This 2-component crackling system creates very fine cracks as you can see on old porcelain.
Apply step 1/2 to the surface you want to embellish. Once step 1/2 dry, apply step 2/2 and rub well on the surface with your fingers. While the step 2/2 dries the cracks appear.
The pattern of the cracks is dependent on the thickness of the two applied layers and the drying time.
The second layer is not waterproof, if
you want to make your project waterproof, varnish it with our Crea Spray varnish (matt 900012/788 or gloss 900012/784) or with Crea Coat (900012/01) or Darwi varnish (724032 matt 724033 gloss)